Okamins Doesnot Tolerate Casting Defects on Turbine Housings.

Some casting defects are not obvious. When we just finish turning the bore of turbine housings, the defects show itself on the surface.

This big size/weight turbine housing is not easy to be casted, as a result, the quality issue happens sometimes. We insists on giving up these housings, while quality is the foundation of our business, we cann’t deliver customer products like these.

IS38 turbine housing

Wax pattern of turbo turbine housing for stainless steel investment casting

Bigger AR stainless steel turbine housing IS38

Turbine housing for TD04L4-11TK3-VG, 9676272680

Crack or shake out ceramic shell of stainless steel investment casting of turbine housing